This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Contact Us
    • Advertise
    • Subscribe
  • NEWS
  • FEATURED
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Thermal Processing Products
    • Top 10 Heat-Treated Holiday Gifts
  • TOPICS
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • COLUMNS
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • Academic Pulse
    • International – Brazil
    • Reshoring Initiative
    • Washington Watch
    • Technical Talk
    • Thermal Processing Matters
  • BLOG
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • DIRECTORIES
    • Equipment Buyers Guide
    • IH Buyers Guide eBook
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • FORGE Buyers Guide
    • FORGE Buyers Guide eBook
    • Take a Tour
  • MULTIMEDIA
    • Podcasts
      • Interviewing the Author
      • Heat Treat Technical Talk
    • Videos
    • Webinars
    • eBooks
  • EVENTS
    • Meetings & Trade Shows
    • Heat Treat Show
    • Heating & Cooling
  • CE CENTER
  • MORE
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • FORGE Magazine
    • Market Research
    • Custom Content & Marketing Services
Home » Keywords: » oxidation

Items Tagged with 'oxidation'

ARTICLES

Industrial Heating Industry News

Tool Manufacturer Orders Retort Furnace

February 2, 2021
No Comments

SECO/WARWICK will deliver a retort furnace with vacuum purging for oxidation to a tool manufacturer. The furnace for the oxidation process operates under a nitrogen and hydrogen mix and then under steam. It will be adjusted to the individual needs of the tool manufacturer, providing the appropriate final hardness and color of the workpieces. The retort furnace, which will also enable tempering after vacuum purging, will be designed with a customized heating chamber so that it is compatible with the tooling used in the production process and so that the process itself is safe and repeatable. 


Read More
Wind-energy Turbines at Sunset
Heat & Corrosion Resistant Materials/Composites

Engineering Strength: Oxide Dispersion for Bulk Alloys

Hannah Diorio-Toth
December 5, 2017
No Comments
Carnegie Mellon University (CMU) researchers are answering the need for heat-tolerant materials by developing a new way to strengthen metals using oxide particles.
Read More
Advanced Steel Parts
Heat & Corrosion Resistant Materials/Composites

Oxidation Behavior of Commercial High-Temperature Alloys

Bo Jönsson Alla Westerlund
March 8, 2017
One Comment

The behavior of high-temperature alloy constructions used in oxidizing environments is important for processes like PM sintering and thermal processing of advanced steels.


Read More
Linn High Therm GmbH protective gas chamber furnace
Products

Protective Gas Chamber Furnace

February 11, 2016
No Comments

The protective gas chamber furnace includes a gas-tight muffle for heat-treatment processes under protective gas atmosphere up to 1050°C (1922°F).


Read More
High-temperature oxidation manifesting itself as surface and subsurface porosity
The Heat Treat Doctor®

High-Temperature Oxidation – A Case Study

Daniel Herring
Daniel H. Herring
February 10, 2016
No Comments

The effect of hydrogen on aluminum alloys can manifest itself in a phenomenon known as high-temperature oxidation (HTO), also known as high-temperature deterioration (HTD).


Read More
RA 602 CA® tube assembly
Heat & Corrosion Resistant Materials/Composites

RA 602 CA®: An Alloy for the Most Extreme Temperatures

Marc Glasser
September 8, 2015
One Comment

RA 602 CA® – also known as 602 CA® and NiCroFer 6025, which are trademarks of VDM – is a relatively new heat-resistant alloy with excellent creep strength at very high temperatures and oxidation resistance up to 2250°F (1232°C).


Read More
ih0914-hcrmc-lead-422.jpg

Selecting an Appropriate Heat-Resistant Alloy

Marc Glasser
April 10, 2015
No Comments

The first factor in choosing a heat-resistant alloy for a particular application is its temperature limit. 


Read More
Subscribe For Free!
  • eMagazine Issues
  • eNewsletters
  • Manage My Preferences
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

figure one

Bainite and How it is Formed

Hardness Measurement Method

Finding the Right Case-Hardness Measurement Method

decarbonization part 3

Decarbonization Options for Industrial Process Heating (Part 3)

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

IH Classifieds

Get our new eMagazine delivered to your inbox every month.

Stay in the know on the latest thermal-processing news and information.

SUBSCRIBE TODAY!
  • Want More?
    • Industry News
    • eNewsletter
    • Connect
  • Resources
    • Industry Links
    • Manufacturing Group
    • List Rental
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY
    • UPDATE MY PREFERENCES

Copyright ©2023. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing