This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Contact Us
    • Advertise
    • Subscribe
  • NEWS
  • FEATURED
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Thermal Processing Products
    • Top 10 Heat-Treated Holiday Gifts
  • TOPICS
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • COLUMNS
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • Academic Pulse
    • International – Brazil
    • Reshoring Initiative
    • Washington Watch
    • Technical Talk
  • BLOG
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • DIRECTORIES
    • Equipment Buyers Guide
    • IH Buyers Guide eBook
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • Take a Tour
  • MULTIMEDIA
    • Podcasts
      • Interviewing the Author
      • Heat Treat Technical Talk
    • Videos
    • Webinars
    • eBooks
  • EVENTS
    • Meetings & Trade Shows
    • Heat Treat Show
    • Heating & Cooling
  • CE CENTER
  • MORE
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • FORGE Magazine
    • Market Research
    • Custom Content & Marketing Services
Home » Keywords » steel

Items Tagged with 'steel'

ARTICLES

Jominy End-Quench Test
Reader Favorite | Materials Characterization & Testing

Understanding the Jominy End-Quench Test

Classic steel hardenability testing
James Marrow
July 16, 2019
No Comments

The Jominy end-quench test is used to measure the hardenability of a steel, which is a measure of the capacity of the steel to harden in depth under a given set of conditions. This article considers the basic concepts of hardenability and the Jominy test.


Read More
Stacks of Cylindrical Steel Parts
Melting/Forming/Joining

Modeling, Simulation and Visualization Capability for Steel Manufacturing

David R. Forrest Theresa Miller Lori Diachin Aaron Fisher Daniel Waters Chenn Zhou Armin Silaen Tyamo Okosun
November 9, 2017
No Comments
Scientists with high-performance computing (HPC) modeling, simulation and visualization capabilities at the Department of Energy's national laboratories are partnering with U.S. industries to optimize blast furnaces in order to reduce emissions and energy use.
Read More
Xiaoqing Cai with Dean Hoffman and Richard Sisson
Induction Heat Treating

Comparative Analysis of Induction and Furnace Tempering

Xiaoqing Cai Richard D. Sisson Jr.
December 2, 2016
No Comments

The CHTE at Worcester Polytechnic Institute (WPI) in Massachusetts has been working on a one-of-a-kind research project aimed at better understanding the mechanical properties and microstructural features of steels that have been gas tempered and induction tempered.


Read More
Debbie Aliya

Evaluating Fire Damage in Buildings (part 1)

Debbie
Debbie Aliya
November 14, 2016
No Comments

One of the most interesting and exciting projects I ever worked on was the evaluation of a large industrial building constructed in the mid-1920s that had a fire in the early part of this current century.


Read More
CarbTool is simulation software that helps heat treaters predict the carubirzation performance of a variety of steels
Industrial Gases/Combustion

CarbTool – Leading the Way in Case-Depth Simulations

Lei Zhang Richard D. Sisson Jr.
October 6, 2016
No Comments

At the Center for Heat Treating Excellence (CHTE) at Worcester Polytechnic Institute (WPI) in Massachusetts, researchers are perfecting carbon-concentration profile predictions through enhancements to CarbTool©, its simulation software.


Read More
Industrial Heating Products
Products

Metal Removal Fluid

May 10, 2016
No Comments

HOCUT 4440 is formulated for the automotive, general machining and grinding markets for use on ferrous metals such as cast iron, ductile iron and steels.


Read More
Flexible vacuum processing cell including oil-quenching furnace
Heat Treating

Vacuum Oil Quenching: Applications and Unique Properties

Philippe Lebigot
January 8, 2016
No Comments

Hardening of steel is a major operation in heat treatment.


Read More
Powder metallurgy utilizes advanced compaction techniques and new alloy systems to optimize mechanical performance of the resulting powder-metallurgy (PM) part
Sintering/Powder Metallurgy

Lower-Alloy Steels for High-Performance PM Applications

Bruce Lindsley Patrick King Sunil Patel Suresh Shah Jerry Falleur
December 2, 2015
One Comment

Powder metallurgy is a continually evolving technology utilizing advanced compaction techniques and new alloy systems to optimize mechanical performance of the resulting powder-metallurgy (PM) part.


Read More
Two dies during plasma nitriding viewed through the port window with intense glow around the central anode
Cover Feature | Vacuum/Surface Treatment

Improving Performance of Stamping Dies with Ion/Plasma Nitriding

E. Rolinski M. Woods T. Damirgi G. Sharp
November 3, 2015
No Comments

The need for lighter and safer vehicles increases the demand for stronger steels in automotive bodies. Aerospace components have many of the same demands but on a more rigidly controlled level with a wider variety of materials.


Read More

Alabama Company Orders Box Furnace

October 14, 2015
No Comments

Thermcraft Inc. of Winston-Salem, N.C., received an order for a large box furnace from an Alabama-based company that remanufactures steel mill rolls.


Read More
More Articles Tagged with 'steel'
Subscribe For Free!
  • eMagazine Issues
  • eNewsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

042122-coffee-web.jpg

Coffee Grounds Used to Make Green Steel

042722-MP-web.jpg

Construction Begins on Rare-Earth Manufacturing Facility in Texas

Industrial Heating Industry News

Steelmaker in India Orders Blast Furnace

FORGE rfp logo

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse the industry's comprehensive buying resource for locating equipment suppliers for nearly any high-temperature thermal preocessing equipment system

Find Suppliers

Events

June 15, 2022

Process Heating & Cooling Show

heating and cooling showThe Process Heating & Cooling Show is a conference and tradeshow that will bring together industrial manufacturing and engineering professionals to learn, connect, share and explore all things related to the process heating and cooling industries.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

IH Classifieds

Get our new eMagazine delivered to your inbox every month.

Stay in the know on the latest thermal-processing news and information.

SUBSCRIBE TODAY!
  • Want More?
    • Industry News
    • eNewsletter
    • Connect
  • Resources
    • Industry Links
    • Manufacturing Group
    • List Rental
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2022. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing