This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Sign Out
  • My Account
Industrial Heating logo
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Contact Us
  • NEWS
  • FEATURED
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Thermal Processing Products
    • Top 10 Heat-Treated Holiday Gifts
  • TOPICS
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • COLUMNS
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • Academic Pulse
    • International – Brazil
    • Reshoring Initiative
    • Washington Watch
    • Technical Talk
    • Thermal Processing Matters
  • BLOG
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • DIRECTORIES
    • Equipment Buyers Guide
    • IH Buyers Guide eBook
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • Take a Tour
    • Cooling Directory
  • MULTIMEDIA
    • Podcasts
      • Interviewing the Author
      • Heat Treat Technical Talk
    • Videos
    • Webinars
    • eBooks
  • EVENTS
    • Meetings & Trade Shows
    • Heat Treat Show
    • Heating & Cooling
  • CE CENTER
  • MORE
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • Market Research
    • Custom Content & Marketing Services
Home » Blogs » Industrial Heating Experts Speak Blog » Debbie Aliya - Failure Analysis

Industrial Heating Experts Speak Blog
Industrial Heating Experts Speak Blog RSS FeedSubscribe

Industrial Heating Blog
Learn from leading experts in the thermal processing industry. Read Industrial Heating’s Expert Speak blogs. Helpful and timely technical information from those who know.
Email
Tweet

Blog Topics

Dan Herring - Heat Treatment

David Pye - Metallurgy

Dan Kay - Brazing

Debbie Aliya - Failure Analysis

George Vander Voort - Metallography

Thomas Joseph - Intellectual Property

Omar Nashashibi – Government

Reed Miller – Thermal Processing

Recent Comments

definitions HT, passivate

Man Care

Brazing of 2205 Duplex Stainless Steel to 7020 & 5083 Aluminum alloy

grain boundary oxidization

Thanks to the Mike or Mikes!

Debbie Aliya - Failure Analysis

This Holiday Season, Celebrate Uncertainty!

Debbie Aliya
Debbie Aliya
December 17, 2014

"We don’t see reality as it is. We see it as WE ARE."


Read More
Debbie Aliya - Failure Analysis

Failure Analysis: Important Definitions

Debbie Aliya
Debbie Aliya
November 3, 2014

In failure-analysis work, we often want to know why the damage happened


Read More
Debbie Aliya - Failure Analysis

How to Look at Microscope Images: Cross Sections (part 2)

Debbie Aliya
Debbie Aliya
July 15, 2014

In a polycrystalline material, which includes the majority of tonnage of commercial metals and even many polymers, there will be a distribution of crystal orientations within even a small cross section.


Read More
Debbie Aliya - Failure Analysis

How to Look at Microscope Images: Cross Sections (part 1)

Debbie Aliya
Debbie Aliya
June 23, 2014

The classical way to reveal a microstructure in commercial metals is to make a cross section.


Read More
Debbie Aliya - Failure Analysis

How to View Microscope Images (part 5)

Debbie Aliya
Debbie Aliya
April 1, 2014

Many of my clients (or occasionally blog readers!) will send me a photo and ask me a question.


Read More
Debbie Aliya - Failure Analysis

How to View Microscope Images (part 4)

Debbie Aliya
Debbie Aliya
March 18, 2014

Last time, in Figure 13, we saw a series of four pieces of pyrite with increasingly numerous individual crystals within the same approximate volume of material.


Read More
Debbie Aliya - Failure Analysis

How to View Microscope Images (part 3)

Debbie Aliya
Debbie Aliya
February 3, 2014

Note the highly superior depth of field and surface detail visible in the SEM image compared to the light microscope.


Read More
Debbie Aliya - Failure Analysis

How to View Microscope Images (part 2)

Debbie Aliya
Debbie Aliya
December 13, 2013

Here's the second part of our series on how to view microscope images.


Read More
Debbie Aliya - Failure Analysis

How to View Microscope Images (part 1)

Debbie Aliya
Debbie Aliya
November 22, 2013

Over the years, it has become more apparent to me that a lot of people do not know how to look at photos from a microscope.


Read More
Debbie Aliya - Failure Analysis

Strength of Material vs. Durability of the Part (part 2)

Debbie Aliya
Debbie Aliya
October 15, 2013

A common source of confusion in doing a failure analysis is figuring out how strong the material was supposed to be.


Read More
Previous 1 2 … 7 8 9 10 11 12 13 14 15 16 Next
Subscribe For Free!
  • Manage My Preferences
  • Online Registration
  • Customer Service

More Videos

Popular Stories

Reed Miller

Gunmaking: Forging the Barrel

082823-Solar-web.jpg

Tool-and-Die Manufacturer Orders Vacuum Furnace

Dan Herring

The Importance of Recessed Braze Fillets (part 3)

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

IH Classifieds

  • Want More?
    • Industry News
    • Connect
  • Resources
    • Industry Links
    • Manufacturing Group
    • List Rental
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY
    • UPDATE MY PREFERENCES

Copyright ©2023. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing