This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Learn from leading experts in the thermal processing industry. Read Industrial Heating’s Expert Speak blogs. Helpful and timely technical information from those who know.
A half century ago (back in the early 1960s) a lot of research work was done by The American Welding Society (AWS) Committee on Brazing and Soldering to determine appropriate criteria for brazing lap joints.
Whenever a gas is introduced into a brazing furnace for a brazing operation, I’m always very concerned about the dew point of that gas because dew point represents moisture in the gas and moisture represents the presence of oxygen.
Recent Comments
Brazing of 2205 Duplex Stainless Steel to 7020 & 5083 Aluminum alloy
grain boundary oxidization
Thanks to the Mike or Mikes!
Indeed, warned means armed. Although it is never...
critical thinking