This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Contact Us
    • Advertise
    • Subscribe
  • NEWS
  • FEATURED
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Thermal Processing Products
    • Top 10 Heat-Treated Holiday Gifts
  • TOPICS
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • COLUMNS
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • Academic Pulse
    • International – Brazil
    • Reshoring Initiative
    • Washington Watch
    • Technical Talk
    • Thermal Processing Matters
  • BLOG
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • DIRECTORIES
    • Equipment Buyers Guide
    • IH Buyers Guide eBook
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • FORGE Buyers Guide
    • FORGE Buyers Guide eBook
    • Take a Tour
  • MULTIMEDIA
    • Podcasts
      • Interviewing the Author
      • Heat Treat Technical Talk
    • Videos
    • Webinars
    • eBooks
  • EVENTS
    • Meetings & Trade Shows
    • Heat Treat Show
    • Heating & Cooling
  • CE CENTER
  • MORE
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • FORGE Magazine
    • Market Research
    • Custom Content & Marketing Services
Home » Blogs » Industrial Heating Experts Speak Blog » Dan Kay - Brazing

Industrial Heating Experts Speak Blog
Industrial Heating Experts Speak Blog RSS FeedSubscribe

Industrial Heating Blog
Learn from leading experts in the thermal processing industry. Read Industrial Heating’s Expert Speak blogs. Helpful and timely technical information from those who know.

Blog Topics

Dan Herring - Heat Treatment

David Pye - Metallurgy

Dan Kay - Brazing

Debbie Aliya - Failure Analysis

George Vander Voort - Metallography

Thomas Joseph - Intellectual Property

Omar Nashashibi – Government

Reed Miller – Thermal Processing

Recent Comments

Brazing of 2205 Duplex Stainless Steel to 7020 & 5083 Aluminum alloy

grain boundary oxidization

Thanks to the Mike or Mikes!

Indeed, warned means armed. Although it is never...

critical thinking

Effect of Heating Rates on Distortion/Fracture of Assemblies Being Brazed

Dan Kay
Dan Kay
October 1, 2009
No Comments
Question: We are using a heating rate of approximately 25-30°F per minute in our atmosphere retort-type brazing furnace for low-carbon steel assemblies we are brazing. Each assembly consists of a
Read More

Can I Braze Metals to Ceramic?

Dan Kay
Dan Kay
September 3, 2009
3 Comments
Brazing is a highly versatile joining technique that can even allow metals to be permanently bonded to certain structural ceramic materials.
Read More

Fluxes For Use When Vacuum Brazing

Dan Kay
Dan Kay
July 30, 2009
No Comments
Question: I was asked to find a flux for use when we are vacuum brazing. Is there any such product on the market today? Do they work?Answer: No, there are
Read More

Brazing Copper to Stainless Steel in Vacuum

Dan Kay
Dan Kay
June 25, 2009
No Comments
Question: We're having trouble brazing a pure copper part to 304L stainless in a vacuum furnace with silver-based brazing filler metal. The stainless comes out a dark color, and the
Read More

Concerns with Brazing 409 Stainless

Dan Kay
Dan Kay
May 28, 2009
No Comments
Question: Our customer used to send us assemblies made from 304 stainless steel for us to furnace braze, using pure copper as the brazing filler metal. The customer now wants
Read More

Vertical Test Specimen for Furnace Brazing (Part 2)

Dan Kay
Dan Kay
May 14, 2009
2 Comments
The VTS provides a unique way to determine exactly what kind of braze clearances can be tolerated in your particular furnace with your particular base metals and BFMs.
Read More

Vertical Test Specimen for Furnace Brazing

Dan Kay
Dan Kay
May 7, 2009
No Comments
Furnace brazing is a common brazing process around the world, and I have witnessed many brazing furnaces in action in many countries – from here to mainland China.
Read More

Fillets in Brazing (Part 3)

Dan Kay
Dan Kay
April 30, 2009
No Comments
Today’s blog concludes our discussion on fillets in brazing.
Read More

Fillets in Brazing (Part 2)

Dan Kay
Dan Kay
April 23, 2009
No Comments
It was shown in last week's blog that brazing fillets can be a greatly misunderstood phenomenon.
Read More

Fillets in Brazing (Part 1)

Dan Kay
Dan Kay
April 16, 2009
No Comments
Brazing fillets can be a greatly misunderstood phenomenon in brazing.
Read More
Previous 1 2 … 10 11 12 13 14 15 16 17 18 Next
Subscribe For Free!
  • eMagazine Issues
  • eNewsletters
  • Manage My Preferences
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

figure one

Bainite and How it is Formed

Hardness Measurement Method

Finding the Right Case-Hardness Measurement Method

decarbonization part 3

Decarbonization Options for Industrial Process Heating (Part 3)

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

IH Classifieds

Get our new eMagazine delivered to your inbox every month.

Stay in the know on the latest thermal-processing news and information.

SUBSCRIBE TODAY!
  • Want More?
    • Industry News
    • eNewsletter
    • Connect
  • Resources
    • Industry Links
    • Manufacturing Group
    • List Rental
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY
    • UPDATE MY PREFERENCES

Copyright ©2023. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing