This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Contact Us
    • Advertise
    • Subscribe
  • NEWS
  • FEATURED
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Thermal Processing Products
    • Top 10 Heat-Treated Holiday Gifts
  • TOPICS
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • COLUMNS
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • Academic Pulse
    • International – Brazil
    • Reshoring Initiative
    • Washington Watch
    • Technical Talk
  • BLOG
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • DIRECTORIES
    • Equipment Buyers Guide
    • IH Buyers Guide eBook
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • Take a Tour
  • MULTIMEDIA
    • Podcasts
      • Interviewing the Author
      • Heat Treat Technical Talk
    • Videos
    • Webinars
    • eBooks
  • EVENTS
    • Meetings & Trade Shows
    • Heat Treat Show
    • Heating & Cooling
  • CE CENTER
  • MORE
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • FORGE Magazine
    • Market Research
    • Custom Content & Marketing Services
Home » Authors » Dr. Bryan Webler

Dr. Bryan Webler

Assistant Professor of Materials Science and Engineering, Carnegie Mellon University

Articles

ARTICLES

ih1119-academic-900
ACADEMIC PULSE

Machine Learning for Nonmetallic Inclusions

Dr. Bryan Webler
November 11, 2019
No Comments

Process metallurgists (like me) use math, physics and chemistry to describe what happens during metal manufacturing. Other researchers use math, statistics and computer science to study and optimize manufacturing at a larger scale.


Read More
ih0819-ap-image-900
ACADEMIC PULSE

Developing Alloys for AM Processes

Dr. Bryan Webler
August 7, 2019
No Comments

Much of the current research and development in additive manufacturing is devoted to making parts from just a few specific alloy compositions.


Read More
Dr. Bryan Webler
ACADEMIC PULSE

Studying Automotive-Steel Microstructures

Dr. Bryan Webler
May 3, 2019
No Comments

Despite its history and ubiquitous presence as an infrastructure material, steels remain a complex material system with many persisting research questions.


Read More
ih0219-ap-graphic-900
ACADEMIC PULSE

Reduction of Metal AM Melt-Pool Bead-Up

Dr. Bryan Webler
February 14, 2019
No Comments

Additive manufacturing (AM) is changing how we think about making parts from metal.


Read More
Subscribe For Free!
  • eMagazine Issues
  • eNewsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

lead

Applying Through-Process Temperature Monitoring in Continuous Furnaces

Industrial Heating Industry News

Steel Dynamics to Build, Operate Aluminum Flat-Rolled Mill

Industrial Heating Industry News

MTI Educational Foundation Awards Scholarship

Clear Seas Research
FORGE rfp logo

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse the industry's comprehensive buying resource for locating equipment suppliers for nearly any high-temperature thermal preocessing equipment system

Find Suppliers

Events

September 15, 2022

Annealing Furnace Optimization in the Cloud

Join us to hear how a cloud-based data management and advisory system conserves resources by moving away from a “set it and forget it” mode.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

IH Classifieds

Get our new eMagazine delivered to your inbox every month.

Stay in the know on the latest thermal-processing news and information.

SUBSCRIBE TODAY!
  • Want More?
    • Industry News
    • eNewsletter
    • Connect
  • Resources
    • Industry Links
    • Manufacturing Group
    • List Rental
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2022. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing