This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Contact Us
    • Advertise
    • Subscribe
  • NEWS
  • FEATURED
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Thermal Processing Products
    • Top 10 Heat-Treated Holiday Gifts
  • TOPICS
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • COLUMNS
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • Academic Pulse
    • International – Brazil
    • Reshoring Initiative
    • Washington Watch
    • Technical Talk
  • BLOG
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • DIRECTORIES
    • Equipment Buyers Guide
    • IH Buyers Guide eBook
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • Take a Tour
  • MULTIMEDIA
    • Podcasts
      • Interviewing the Author
      • Heat Treat Technical Talk
    • Videos
    • Webinars
    • eBooks
  • EVENTS
    • Meetings & Trade Shows
    • Heat Treat Show
    • Heating & Cooling
  • CE CENTER
  • MORE
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • FORGE Magazine
    • Market Research
    • Custom Content & Marketing Services
Home » Authors » E. Rolinski

Articles by E. Rolinski

ih1120-vst-fig1-900
Vacuum/Surface Treating

Enhancing Automotive Stamping-Die Performance with Plasma Nitriding

Whether with advanced high-strength steel (AHSS) or mild steel, many automotive parts need to be stamped. Dies for stamping those parts need to be optimized, and that drives the need for surface treatments.
E. Rolinski M. Woods
November 11, 2020
No Comments

Metallurgists are developing new steels to assist automotive engineers in designing better trucks, cars and SUVs.


Read More
Industrial Heating Web Exclusives
Web Exclusive

Nitriding of Powder-Metal Components

E. Rolinski M. Woods
May 29, 2019
No Comments

The application of ion/plasma nitriding to powder-metal (PM) products is recommended over the gas nitriding method. Ion/plasma nitriding results in surface hardening while gas nitriding causes unintended through-nitriding, making the treatment not suitable for a majority of engineering components made of PM.


Read More
ih0319-vst-fig2-900
VACUUM/SURFACE TREATING

Engineering the Surface

The importance of early-stage design decisions for enhancing surface properties of steel and cast-iron components with nitriding and nitrocarburizing cannot be overstated.
E. Rolinski M. Woods
March 13, 2019
No Comments

Modern designing of mechanical components and tools should take under consideration their intrinsic stresses and surface condition.


Read More
Two dies during plasma nitriding viewed through the port window with intense glow around the central anode
Cover Feature | Vacuum/Surface Treatment

Improving Performance of Stamping Dies with Ion/Plasma Nitriding

E. Rolinski M. Woods T. Damirgi G. Sharp
November 3, 2015
No Comments

The need for lighter and safer vehicles increases the demand for stronger steels in automotive bodies. Aerospace components have many of the same demands but on a more rigidly controlled level with a wider variety of materials.


Read More
IH0114-VST-lead-422.jpg
FEATURE | Vacuum/Surface Treating

Heating in Plasma Nitriding Furnaces

E. Rolinski G. Sharp M. Woods J. Machinski
January 7, 2014
No Comments

Heating of loads in modern plasma nitriding furnaces is carried out by a combination of the radiative heat transfer from the wall or furnace resistance heaters and heat transfer from the glow discharge. We will look at the effect of the workpiece emittance on its temperature.


Read More

Plasma, Gas Nitriding and Nitrocarburizing for Engineering Components and Metal-Forming Tools

E. Rolinski T. Damirgi G. Sharp
May 3, 2012
One Comment
Wear, corrosion and fatigue properties are strongly dependent on surface quality and its modifications. Thermochemical methods such as gas and plasma nitriding allow for enhancement of these properties in most severely loaded (mechanically and/or chemically) applications without causing any changes in dimensions of the treated objects.
Read More
Subscribe For Free!
  • eMagazine Issues
  • eNewsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Industrial Heating Industry News

Top Steel Producers in 2021

flue gas

Better Flue Gas Analysis Improves Combustion Control

Industrial Heating Industry News

Watlow to Acquire Eurotherm from Schneider Electric

FORGE rfp logo

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse the industry's comprehensive buying resource for locating equipment suppliers for nearly any high-temperature thermal preocessing equipment system

Find Suppliers

Events

June 28, 2022

Sectioning of Complex Components for High-Volume Metallographic Sample Preparation

The first step for metallographic preparation is sectioning the sample to a manageable size. Join us as we discuss Struers’ Magnutom 5000, Premium cut off wheels, and other solutions for high-volume metallographic sectioning.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

IH Classifieds

Get our new eMagazine delivered to your inbox every month.

Stay in the know on the latest thermal-processing news and information.

SUBSCRIBE TODAY!
  • Want More?
    • Industry News
    • eNewsletter
    • Connect
  • Resources
    • Industry Links
    • Manufacturing Group
    • List Rental
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2022. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing