This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This article presents the vacuum-carburizing technology of Pyrowear® Alloy 53 steel. It discusses the methods of establishing different carbon concentration profiles in a layer and their influence on the hardness profile.
This article describes the newest achievements in the heat treatment of diesel-engine fuel-injection nozzles made of hot-working tool steel. Different methods of improving surface properties have been applied by means of vacuum carburizing and vacuum nitriding, which is especially suitable for elements characterized by difficult shape geometry such as blind holes. Variable process parameters have been considered in terms of sequence and temperature as well as their influence on surface microstructure, hardness and case-layer uniformity.
HPGQ vacuum furnaces are commonly used for heat treating high-, medium- and low-alloy steel tools, HSLA steel products and for individual applications of low-pressure (vacuum) carburizing (LPC) technology.
This article discusses the new generation, single-chamber vacuum furnace with a high-pressure gas-quenching system (HPGQ) able to quench with an efficiency better than that achieved in furnaces with a separate gas-quenching chamber (cold chamber) and comparable to the efficiency of oil systems