This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Bodycote, the world’s largest provider of specialist thermal-processing services, announced the opening of a new facility in Syracuse, N.Y. The 60,000-square-foot facility is operational and offers a wide range of heat-treatment processes, including vacuum heat treating, atmospheric carburizing, low-pressure carburizing, carbonitriding, ferritic nitrocarburizing, nitriding and aluminum heat treating. The site is working toward securing all major OEM approvals as well as Nadcap accreditation, which it is on the way to achieving.
Industrial Heating in cooperation with SECO/WARWICK
January 12, 2021
Editor’s note: The following is an edited (for length) transcription of an interview between SECO/WARWICK’s Tom Hart and Dan Herring, The Heat Treat Doctor. It was part of the company’s E-Seminar held in September 2020.