This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Quintus Technologies will supply a hot isostatic press (HIP) to the 10,000-square-foot metal additive-manufacturing (AM) center recently opened by Sintavia LLC in Davie, Fla.
Arcam, a supplier of additive-manufacturing equipment based in Sweden, announced that its subsidiary AP&C of Montreal will add capacity by building a new powder manufacturing plant.
It is well known that accurate measurement of any heat-treating atmosphere can have a significant effect on the quality and process yield of heat-treated components.
Researchers at Missouri University of Science and Technology will collaborate with Honeywell Federal Manufacturing & Technologies on a five-year project to perform material analysis for the selective laser melting (SLM) process in a metal powder bed.
Norsk Titanium will partner with Bosch Rexroth AG to provide customized drive and control solutions for Norsk’s patented rapid plasma deposition (RPD) machines in Europe and to fulfill orders bound for the U.S. market.