SLM Solutions (Germany) and Safran Landing Systems (France) collaborated to test SLM Solutions’ selective laser-melting AM technology, otherwise known as laser-beam powder-bed fusion (PBF-LB). The component was redesigned for metal AM, which enabled time saving in the whole process and significant weight reduction of approximately 15%.