There is so much development going on with PM/AM that it is almost not news when new powders are developed. Rusal America has added new powders for AM applications comprised of four traditional Al-Si-based casting alloys and five specialty alloys designed for use in the aerospace and automotive industries. Composition is optimized to maximize properties and printability while minimizing material cost.