With the push to electrify vehicles and the need for renewable-energy storage batteries, much work is being done in battery development. One such effort has resulted in a hard-carbon negative electrode material requiring a lower heat-treatment temperature of 1500°C.
More work needs to be done, but a sodium-ion battery using this carbon electrode material would result in a 19% increase in energy density over lithium-ion batteries. Here's the story.