The 2021 Ford Bronco is getting its steel from a mill in Alabama. AM/NS Calvert – a joint venture between ArcelorMittal and Nippon Steel – is producing a new ultra-high-tech steel specifically for the vehicle. Fortiform 980 GI was developed by ArcelorMittal in conjunction with Ford.