This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
At its halfway point, a project to industrialize additive manufacturing (IDAM) has resulted in a new metal powder, DP 600. GKN Powder Metallurgy, one of 12 project partners, says that its dual-phased steel is a good candidate for several structural automotive applications because the mechanical properties can be enhanced with heat treatment.