This article takes a thorough look at adopting AM with a particular focus on laser powder-bed fusion. It describes the uncertainties and risks along with the ability to innovate. The author notes that “thermal postprocessing — stress relief, heat treatment and/or hot isostatic pressing (HIP) — is critical for achieving the desired mechanical properties.”
magEzine news
Industrializing Additive Manufacturing

May 20, 2020
No Comments