A U.K.-based company is making additively manufactured titanium handlebars for high-performance cycles. Metron Additive Manufacturing uses GE Additive Arcam electron-beam-melting (EBM) technology to manufacture the handlebars, which have been on bikes that won world championships and Olympic gold medals.