The evidence is in. That cool-looking Apple Card is made from 90% titanium and 10% aluminum. Others speculate the alloy is likely Ti6Al4V, which would mean it is actually 90% Ti, 6% Al and 4% V.
magEzine news
From what is the Apple Card made?

The evidence is in. That cool-looking Apple Card is made from 90% titanium and 10% aluminum. Others speculate the alloy is likely Ti6Al4V, which would mean it is actually 90% Ti, 6% Al and 4% V.