Sintavia LLC, an independent metal additive manufacturer, acquired QC Laboratories Inc. (QC Labs), a nondestructive testing (NDT) services company based in Hollywood, Fla. The acquisition enhances Sintavia’s NDT capabilities for commercial aerospace applications, particularly with respect to surface-finish conformance testing. QC Labs specializes in radiographic (X-ray and gamma), fluorescent-penetrant, ultrasonic, magnetic-particle and eddy-current inspections. The company holds approvals for these processes from Honeywell Aerospace, Lockheed Martin, General Electric, Collins Aerospace, Pratt & Whitney, Cessna, Eaton, Aerojet Rocketdyne and Rolls-Royce.
It is expected that QC Labs, which is Nadcap- and AS9110-certified, will operate as a stand-alone subsidiary of Sintavia. The company has three locations: Hollywood and Orlando, Fla., and Cincinnati, Ohio.