Tenova LOI Thermprocess received an order from U.S. Steel Kosice, a Slovakian steel producer and fully integrated metallurgical plant, for an annealing and coating line (ACL) for dynamo steel strips. Tenova will supply the complete ACL, including a heat-treatment furnace, drying oven and the associated electrical, instrumentation and control technology. The plant will use the ACL to produce non-grain-oriented electrical steel. The contract scope includes engineering, turnkey delivery of all equipment and supervision of the assembly and commissioning.
U.S. Steel Kosice is a wholly owned subsidiary of U. S. Steel.