Space doesn’t allow us to discuss the parts in detail, but Bugatti is using AM for a number of functional parts. These include: titanium brake caliber, active spoiler bracket made of titanium, motor bracket (AlSi10Mg) with integral cooling, front axle differential housing and cylinder-head cam covers.
magEzine news
AM Parts for your Bugatti

Source: Bugatti
May 17, 2019
No Comments