Nucor Corp. acquired certain assets from Century Tube LLC. Based in Madison, Ind., Century Tube supplies carbon steel tubing for automotive and other mechanical and structural applications. The company offers round, square, rectangular, oval and other special welded shapes of mechanical steel tubing. Century Tube, which also supplies induction heat-treated tubes for automotive applications, operates from a 280,000-square-foot facility located on 33 acres.