An Italian company has developed a solution for bucket wheel excavator teeth. Using its forging technology, Berco – part of the Forged Technologies group of thyssenkrupp Components Technology – created more-resistant, lightweight and higher-performance bucket wheel excavator teeth. The use of high-quality steel and advanced mechanical superficial heat treatment provides extended product life.
The company also designed a solution for faster connection to the bucket to reduce needed replacement work in the field. Read more about it.