Swansea University in cooperation with Tata Steel and WMG are working on the “virtual factory.” Their solution combines physical testing and computational modelling to rapidly “test” hundreds of small-scale samples. Tests include resistance to corrosion, strength, electrical and mechanical properties. Models allow the test data to predict the best alloys, which will then undergo further production/testing.
Click here to learn more.