This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Fiat Chrysler Automotive has recalled about 18,000 2018 and 2019 Jeep Wrangler JLs for welds that could lead to a “crash without prior warning.” No accidents or injuries have been reported, and it is expected that the defect will be found on 4% (720) of the recalled vehicles.
Share This Story
You must login or register in order to post a comment.
Report Abusive Comment