No. 1045 is a 1250°F (677°C) horizontal-airflow cabinet oven that can be used for heat treating. Workspace dimensions measure 38 inches wide x 38 inches deep x 38 inches high. A 2,000-CFM, 2-HP recirculating blower provides horizontal airflow. The oven features 12-inch-thick insulated walls comprised of 2 inches of 2300°F ceramic blanket and 10 inches of rockwool. It includes all safety equipment required by National Fire Protection Association Standard 86 for gas-heated equipment as well as a digital indicating temperature controller.