In spite of everything that makes titanium a wonder metal, it is very expensive to produce due to a complex 40-stage process. With this in mind, FAST-forge turns titanium-alloy powders into near-net-shape components (with wrought properties) in two steps. This new process could reduce the cost of parts by 50% and increase the number of parts that can be produced from titanium.

Learn more about it here.