This brief article discusses the relationship between 3D printing and heat treatment. The heat treatment of some 3D-printed parts has been shown to dramatically increase their strength and stiffness. It is also demonstrated that 3D printing can advantageously affect the properties of heat-treated parts and can be assist the manufacturing process.