Thermbond 7200 Series can substantially reduce the cost of most furnace repairs through its ability to provide consistent properties regardless of installation method. It provides excellent and consistent properties with all common installation methods – casting, pumping, gunning, ramming and shotcreting. Thermbond 7200 Series is mixed with water for casting or pumping, with 7200 Liquid for gunning or ramming, or with 7200 Accelerator for shotcreting. Only two different liquids are required for all five major installation methods, and the amount of liquid is roughly 5% by volume of the dry mix. Depending on the installation configuration, thickness, lining condition and geometry, Thermbond 7200 Series can be fired in at up to 200°C per hour with no holds.