There have been numerous complaints that a rifle manufactured by Savage Arms, the 10ML-II muzzleloader, exploded, burst, split or cracked. Martin Crimp, a Michigan State University metals expert who examined a 10ML-II that exploded and caused a hunter to lose multiple fingers in 2009, said that the barrel of that gun was “metallurgically defective.”