THERMA quenching oils are formulated exclusively from Group III, highly refined base oils to ensure safe and efficient use. Advantages include: increased flash point to reduce fire risk; decreased Sulphur content and aromatic compounds; and decreased pressure on filtration systems. The THERMA range is available in different qualities (cold, semi-hot and warm oils) and covers all quench types (batch, vacuum and open furnaces).