Ipsen supplied a TITAN H6 vacuum furnace with 6-bar gas quenching to Diamond Heat Treat of Rockford, Ill. Diamond Heat Treat will use the furnace to expand its capabilities. The furnace features a 36- x 48- x 36-inch (915- x 1,220- x 915-mm) work zone with a 3,000-pound (1,361-kg) load capacity. It is capable of operating at temperatures of 1000-2400°F (538-1316°C) with ±10°F (±6 °C) temperature uniformity. Ipsen will also provide hands-on support for installation, start-up supervision and personnel training.