As those of us in a high-temperature field know well, metals expand when heated due to thermal expansion. This can create a problem for machines operating in high-temperature environments. A team of researchers in Japan have discovered a material that shrinks a record-breaking 6.7% when heated. The goal would be to use these materials to develop composites with no expansion or contraction when heated.