Lindberg/MPH shipped a tube furnace with a temperature range of 932-2192°F (500-1200°C) that will be used for a laboratory application. Chamber dimensions are 1 inch wide x 12 inches long. The furnace includes a mild-steel hinged-shell design to allow for ease of use. Vacuum-formed ceramic-fiber insulation with embedded heating elements is used for quick heat-up and low heat storage. The unit, which can be mounted horizontally or vertically, is available in either 120V or 240V rated at 960 watts.