Nutec Bickley received an order from Specialty Ring Products (SRP) for two gas-fired rotary-hearth furnaces. The units, which have an operating temperature range of 1500-2150°F (815-1175°C), will process steel alloy, Inconel and titanium products at SRP’s facility in Bensalem, Pa. The furnace design incorporates the latest technology in combustion equipment and controls. The units also include Nutec Bickley’s special ultra-large ceramic-fiber modules, which eliminate hot spots.