After completing an intensive three-day audit, Solar Atmospheres Southeast announced its addition to the Boeing approved-processor listing. The Greenville, S.C., facility now has an approved scope of processing includes the following specifications:

  • BAC 5613 – Heat Treatment of Titanium and Titanium Alloys
  • BAC 5616 – Heat Treatment of Nickel-Base and Cobalt-Base Alloys
  • BAC 5619 – Heat Treatment of Corrosion Resistant Steel

With thermal processing in furnaces ranging from those suited for small lots and development cycles to a 6.5-foot-diameter x 24-foot-long vacuum chamber capable of processing up to 50,000-pound loads with a maximum temperature of 2400°F, Solar Atmospheres is backed by AS9100 and Nadcap quality systems.