For fuel efficiency, the automotive industry is always looking for ways to save weight. Renault Trucks’ engineers and designers are using AM to boost the performance of its engines. They have been able to save 25% of the weight and reduce the number of parts by 25% as well, which amounts to 200 fewer parts.