Dorssers Inc. purchased two SECO/WARWICK pit-style air temper furnaces for its manufacturing facility in Blenheim, Ontario. Dorssers Inc. manufactures dies with a wide range of specifications. The pellet dies are large-diameter, hardened steel dies with a multitude of holes gun-drilled for compressing various feedstocks. The environment is harsh, so exact heat treating is vital. The two electric furnaces, which feature a heavy-duty industrial design for uniform convective heating, will be used to temper these dies.
Dorssers Installs Two Pit Tempering Furnaces
January 2, 2017
No Comments