This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
magEzine News
Earliest Heat Treatment?
October 26, 2016
Recent research indicates that stone-age humans in South Africa used heat to treat stones to make them less fracture tough and harder. Using an NDT technique, researchers determined that 90% of silcrete tools were heat treated. Interested in learning more?