Bodycote announced that its new plant in Greenville, S.C., is open for business. The facility, which is expected to receive Nadcap accreditation by the end of the year, is ready to process metal and alloy parts that require brazing or vacuum heat-treating services. The new Greenville plant will primarily serve the southeast region’s manufacturers and their supply chains in the aerospace, defense, energy and medical industries. Bodycote plans to offer additional services from the facility in the future in response to customer demand.