This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • Home
  • Magazine
    • Digital Magazine
    • Current Issue
    • Archives
  • News
  • Featured
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • IH Economic Indicators
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Top 10 Heat-Treated Holiday Gifts
  • Topics
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • Columns
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • MTI Profile
    • Academic Pulse
    • Heat Treat 5.0
    • International – Brazil
    • Next-Gen Leaders
    • Reshoring Initiative
    • Washington Watch
  • Directories
    • Equipment Buyers Guide
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • Materials Characterization & Testing Equipment Directory
    • Take a Tour
  • More
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • Market Research
    • Custom Content & Marketing Services
    • FORGE Magazine
    • Continuing Education
  • Multimedia
    • Podcasts
    • Videos
    • Webinars
    • Image Gallery
    • eBooks
  • Events
    • Meetings & Trade Shows
    • FNA
    • Heat Treat Show
  • Blog
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • Contact
  • Advertise
  • Subscribe
    • Digital Edition Subscriptions
    • eNewsletter
    • Online Registration
    • Customer Service
Home » Ceralink Offering Fatigue Testing for Metals

You have 0 Articles Left This Month. Register Today for Unlimited Access.

News

Ceralink Offering Fatigue Testing for Metals

February 29, 2016
KEYWORDS fatigue / industrial heating news / metal testing
Order Reprints
No Comments

Ceralink Inc., a service provider in advanced ceramic materials, announced its new offerings in metals testing will include fatigue testing from ambient to 1200°C (2192°F). Ceralink’s recent Materials Testing Lab expansion opened up new opportunities to serve the aerospace industry’s stringent metal testing programs. The Saint Clairsville, Ohio-based company will leverage its experience with precision testing of CMCs and its climate-controlled laboratory to put 16 new MTS Landmark Generation test frames to work on metals. The new offerings include load control high-cycle fatigue and strain-controlled low-cycle fatigue.

You have 0 complimentary articles left.

Register for free today to continue reading!

Already have an account? Sign in here.

Privacy Policy

Related Articles

Ceralink Opens New Materials Testing Facility

Ceralink Expands Materials Testing Facility

Stress-Life Fatigue Testing Basics

Fatigue Testing of Six-Cylinder Diesel Engine Head

Related Products

Atmosphere Heat Treatment: Atmospheres, Quenching, Testing - Vol. 2

Materials Characterization Testing Buyers Guide

Handbook of Materials Selection for Engineering Applications

Related Events

IR Temperature Measurement for Metals Made Simple

Grinding and Polishing of Sample Materials for Microstructural Analysis and Hardness Testing

Related Directories

Epsilon Technology Corp.

Sun-Tec Corp., Detroit Testing Machine

Tinius Olsen Testing

Subscribe For Free!
  • Digital Edition Subscriptions
  • eNewsletters
  • Online Registration
  • Subscription Customer Service

 
More Videos

Popular Stories

1220-WE-fig1

Top 5 Articles of 2020

1220-Belting-lead

Stronger Shaped Wire Belt Stands Up to Rigors of Heat Treating

ih0121-reshoring-900

Moser on Manufacturing

010721-hyperloop

First Passengers Travel Safely on Hyperloop

ih0121-past-photo2-900

Heat Treating: Past, Present and Future

10.29 IH SVT 360X180_NEWcustomcontent

Events

February 16, 2021

Materialographic Preparation of Thermal Spray Coating Samples

With the development of new alloys for coatings, it is even more important than ever to understand how something as generic as sample preparation can affect the evaluation of a coating

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Vacuum Heat Treatment Volume I

Vacuum Heat Treatment Volume I

See More Products

The History of Industrial Heating 1000 BC - Present Day


Industrial Heating Employment Marketplace

Industrial Heating

Cover_Jan8th_144px

January 8, 2021

View More Create Account
  • Resources
    • List Rental
    • eNewsletter
    • Manufacturing Group
    • News
    • Want More?
    • Featured
    • Product / Event
    • Industry Links
    • Connect
    • Privacy Policy
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2021. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing