Morgan Advanced Materials
A range of kiln furniture is made from a new high-performance, nitrite-bonded silicon-carbide material suitable for use at temperatures of up to 2732°F (1500°C). Halsic-N combines the properties of materials such as silicon carbide and silicon nitride in a microstructure that delivers strength, excellent refractory properties and resistance to oxidation and thermal shock. Standard designs include setter plates and beams and supports in a range of sizes. Thermocouple protection tubes made from Halsic-N are ideal for the melting of nonferrous metals such as aluminum and magnesium.