Wisconsin Oven designed and manufactured a gas-fired cold-car industrial batch oven for a custom metal solutions company. The batch oven will be used for stress relieving steel assemblies weighing up to 20,000 pounds at temperatures up to 1250°F. The design provides ease of loading/unloading larger loads with energy-efficient operation. The oven, which has work-chamber dimensions of 10 feet wide x 15 feet long x 10 feet high, utilizes Wisconsin Oven’s patented high-efficiency Expandable Surface design. Limit switches were provided to limit the car travel in both directions, and the temperature is controlled and recorded by a Eurotherm Nanodac programmable recorder/controller.