SECO/WARWICK Corp. received an order to supply a 2-bar vacuum brazing furnace with a graphite hot zone and high-vacuum diffusion pump to Hi TecMetal Group (HTG) of Cleveland, Ohio. The 60- x 60- x 72-inch furnace was customized to meet HTG’s specifications. To eliminate vacuum leaks, the furnace has no rotating vacuum shaft seals and is equipped with SECO/WARWICK’s linear motion clamping ring for the furnace door. The furnace will be installed at HTG’s HiTech Aero facility in Eastlake, Ohio, in the third quarter of 2016. The Eastlake plant is building an 18,000-square-foot addition to house the new equipment and to permit HTG to consolidate its Nadcap welding unit with the Eastlake facility.