Optomec, a leading global supplier of production-grade additive manufacturing systems for 3D-printed metals, signed a distribution agreement with Viwa to represent the Optomec LENS family of 3D metal printers in Mexico and Central America. The turnkey 3D metal printers are used to repair, rework and manufacture high-performance metal components in materials such as titanium, stainless steel and superalloys. The LENS print engine can be integrated with other metalworking machine tools.