SMS group received an order from Royal United Metal and Glass of the United Arab for an inductive billet heater and an extrusion press. The billet heater consists of two induction furnaces, each with a rating of 650 kW. It ensures precision heating in five zones of aluminum extrusion billets with a diameter of 229 mm (9 inches) and a length of up to 1,300 mm (51 inches). Royal United will use the press for the production of aluminum profiles for facades and windows. It extrudes 9-inch billets and has a capacity of approximately 14,000 tons of profiles per year.