Ipsen recently shipped an atmosphere furnace, two temper furnaces, a washer, a loader and a storage table to a commercial heat treater in the Midwest. The batch atmosphere furnace will be used to process parts for the aftermarket automotive and oil and gas industries. The single-chain furnace features a 36- x 48- x 38-inch load size with a 3,500-pound load capacity. It operates at temperatures of 1450-1800°F (788-985°C) and has a quench-oil capacity of 3,500 gallons. The atmosphere furnace also includes: cartridge-type heat-fan assembly, shelf-mounted quench-oil heaters and oil-circulation pump, and safety catwalks for better ease of maintenance.