C.I. Hayes, a Gasbarre Furnace Group Company, recently installed a humpback conveyor belt furnace for bright annealing of stainless steel materials at a facility on the West Coast. The furnace operates with hydrogen atmosphere at a low dew point (-60°F/-76°C range) and has a maximum operating temperature of 2100°F (1149°C).
Humpback Annealing Furnace Installed
July 2, 2015