Knuckleback™ Platinum is a new woven T314 stainless steel conveyor belt used in the final sintering stage in powdered-metal production lines that produce parts for automobiles and other industries. The belt life is significantly extended through a pre-oxidation process that provides surface protection to prevent carbon buildup in the furnace and along the edges of the belt. Field tests have shown that the pre-treating process increases belt life by 25% and reduces operational downtime for belt replacement by more than 18%.