Solar Atmospheres, Southeast officially opened its doors for business in Greenville, S.C. The company brought its first furnace online the first week of May. Other furnaces will continue to be delivered and brought online over the summer months. Full production capability will allow the company to process everything from small lots to 24-foot-long product in a vacuum atmosphere. Solar Atmospheres, Southeast will also provide services ranging from vacuum hardening and annealing to low-pressure carburizing and furnace brazing.